| Manufacturer | Teijin Limited |
| Resin Name | PC/ABS |
| Product Name | Multilon |
| ISO Material Code | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO1183 | Density | ISO1183 | kg/m^3(×10^-3) | 1.26 | - |
Water absorption Water absorption/ISO62 | Water absorption rate (24h in 23℃ water) | ISO62 | % | 0.2 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Vicat softening temperature Vicat softening temperature/ISO306 | Vicat softening temperature (50℃/h 50N) | ISO306 | ℃ | 132 | - |
Deflection Temperature under Load Deflection Temperature under Load/ISO75-1,2 | Deflection temperature under load (1.8MPa) | ISO75-1,2 | ℃ | 126 | - |
Deflection temperature under load (0.45MPa) | ISO75-1,2 | ℃ | 138 | - | |
Linear expansion coefficient (flow) Linear expansion coefficient (flow)/ISO11359-2 | Linear expansion coefficient (parallel) | ISO11359-2 | ×10^-5/℃ | 3 | - |
Linear expansion coefficient (right angle) Linear expansion coefficient (right angle)/ISO11359-2 | Linear expansion coefficient (vertical) | ISO11359-2 | ×10^-5/℃ | 6 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile breaking stress Tensile breaking stress/ISO527-1,2 | Tensile breaking stress (5mm/min) | ISO527-1,2 | MPa | 100 | - |
Tensile strain at break Tensile strain at break/ISO527-1,2 | Tensile breaking strain (5mm/min) | ISO527-1,2 | % | 2 | - |
Tensile Modulus Tensile Modulus/ISO 527-2/1 | Tensile modulus (1mm/min) | ISO 527-2/1 | MPa | 5600 | - |
Bending strength Bending strength/ISO178 | Bending strength (2mm/min) | ISO178 | MPa | 135 | - |
Flexural modulus Flexural modulus/ISO178 | Flexural modulus (2mm/min) | ISO178 | MPa | 5500 | - |
Charpy impact strength Charpy impact strength/ISO179 | Charpy impact strength (unnotched, 23℃) | ISO179 | kJ/m^2 | 32 | - |
Charpy impact strength (notched, 23℃) | ISO179 | kJ/m^2 | 11 | - | |
Charpy impact strength (notched, -30℃) | ISO179 | kJ/m^2 | 10 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Surface resistance Surface resistance/IEC60093 | Surface resistance | IEC60093 | Ω | NaN | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Mold shrinkage rate MD Mold shrinkage rate MD/Company method | Mold shrinkage rate (parallel, 4mmt) | Company method | % | - | |
Mold shrinkage rate TD Mold shrinkage rate TD/Company method | Mold shrinkage rate (vertical, 4mmt) | Company method | % | - | |
MVR MVR/ISO1133 | Melt volume flow rate (250℃ load 5.0kg) | ISO1133 | cm3/10min | 7 | - |
| Key Features |
|---|
Automotive series, glass fiber reinforced, GF20% reinforced |