| Manufacturer | Celanese Corporation |
| Resin Name | PBT |
| Product Name | Crastin |
| ISO Material Code | (PBT+ASA)-GF30 FR(17) |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO 1183 | Density | ISO 1183 | g/cm^3 | 1.55 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Melting point Melting point/ISO 11357-1/-3 | Melting temperature (10℃/min) | ISO 11357-1/-3 | ℃ | 225 | - |
Flammability Flammability/IEC 60695-11-10 | Flammability | IEC 60695-11-10 | class | NaN | 1.5mm |
Glass transition temperature Glass transition temperature/ISO 11357-1/-3 | Glass transition temperature (10℃/min) | ISO 11357-1/-3 | ℃ | 120 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile breaking stress Tensile breaking stress/ISO 527-1/-2 | Breaking Stress | ISO 527-1/-2 | MPa | 115 | - |
Tensile strain at break Tensile strain at break/ISO 527-1/-2 | Breaking Strain | ISO 527-1/-2 | % | 1.7 | - |
Tensile Modulus Tensile Modulus/ISO 527-1/-2 | Tensile Modulus | ISO 527-1/-2 | MPa | 10200 | - |
Charpy impact strength Charpy impact strength/ISO 179/1eA | Notched Charpy impact strength (23℃) | ISO 179/1eA | kJ/m^2 | 7 | - |
Charpy impact strength (23℃) | ISO 179/1eU | kJ/m^2 | 35 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Volume resistivity Volume resistivity/IEC 62631-3-1 | Volume resistivity | IEC 62631-3-1 | Ω・cm | NaN | - |
Surface resistance Surface resistance/IEC 62631-3-2 | Surface resistance | IEC 62631-3-2 | Ω | NaN | - |
Dielectric constant Dielectric constant/IEC 62631-2-1 | Dielectric constant, 100Hz | IEC 62631-2-1 | 4.7 | - | |
Dielectric constant, 1MHz | IEC 62631-2-1 | 4.4 | - | ||
Dielectric loss tangent Dielectric loss tangent/IEC 62631-2-1 | Dielectric loss tangent (100Hz) | IEC 62631-2-1 | E-4 | 54 | - |
Dielectric tangent (1MHz) | IEC 62631-2-1 | E-4 | 203 | - | |
Dielectric Strength Dielectric Strength/IEC 60243-1 | Withstand voltage | IEC 60243-1 | kV/mm | 29 | - |
Tracking resistance Tracking resistance/IEC 60112 | Tracking resistance | IEC 60112 | 325 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
MFR MFR/ISO 1133 | Melt mass flow rate (250℃, 5kg) | ISO 1133 | g/10min | 14 | - |
MVR MVR/ISO 1133 | Melt volume rate, MVR (250℃, 5kg) | ISO 1133 | cm^3/10min | 6.5 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Resin temperature Resin temperature/ | Optimum resin temperature | ℃ | 250 | - | |
Mold Temperature Mold Temperature/ | Optimal Mold Temperature | ℃ | 80 | - | |
Drying conditions Drying conditions/ | Drying temperature | ℃ | 120 | 2 - 4h |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Filler Content Filler Content/ | Filler Content | % | 30 | GF |
| Key Features |
|---|
Flame retardant, low warpage |