| Manufacturer | Celanese Corporation |
| Resin Name | PA612 |
| Product Name | Zytel |
| ISO Material Code | PA612 |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO 1183 | Density | ISO 1183 | g/cm^3 | 1.07 | - |
Water absorption Water absorption/ISO 62 | Balanced water absorption (2mm) | ISO 62 | % | 1.3 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Deflection Temperature under Load Deflection Temperature under Load/ISO 75-1/-2 | Deflection temperature under load (1.80MPa) | ISO 75-1/-2 | ℃ | 63 | - |
Melting point Melting point/ISO 11357-1/-3 | Melting temperature (10℃/min) | ISO 11357-1/-3 | ℃ | 218 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile Yield Stress Tensile Yield Stress/ISO 527-1/-2 | Yield stress (absolutely dry) | ISO 527-1/-2 | MPa | 59 | - |
Yield stress (when humidified) | ISO 527-1/-2 | MPa | 56 | - | |
Tensile strain at break Tensile strain at break/ISO 527-1/-2 | Nominal breaking strain (when completely dry) | ISO 527-1/-2 | % | 38 | - |
Destructive strain (when humidity controlled) | ISO 527-1/-2 | % | 30 | - | |
Tensile Modulus Tensile Modulus/ISO 527-1/-2 | Tensile modulus (when completely dry) | ISO 527-1/-2 | MPa | 2400 | - |
Tensile modulus (when conditioned) | ISO 527-1/-2 | MPa | 1600 | - | |
Flexural modulus Flexural modulus/ISO 178 | Flexural modulus (when completely dry) | ISO 178 | MPa | 2200 | - |
Charpy impact strength Charpy impact strength/ISO 179/1eA | Notched Charpy impact strength (23°C) (when completely dry) | ISO 179/1eA | kJ/m^2 | 4.8 | - |
Notched Charpy impact strength (23°C) (humidified) | ISO 179/1eA | kJ/m^2 | 5.3 | - | |
Charpy impact strength (23℃) (when completely dry) | ISO 179/1eU | kJ/m^2 | N | ||
Charpy impact strength (-30℃) (when completely dry) | ISO 179/1eU | kJ/m^2 | N | ||
Yield Strain Yield Strain/ISO 527-1/-2 | Yield strain (when completely dry) | ISO 527-1/-2 | % | 5 | - |
Yield strain (when humidified) | ISO 527-1/-2 | % | 21 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Resin temperature Resin temperature/- | Optimum resin temperature | - | ℃ | 250 | - |
| Key Features |
|---|
Non-reinforcement |