| Manufacturer | Celanese Corporation |
| Resin Name | PPA |
| Product Name | Zytel |
| ISO Material Code | PA-GF50 |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO 1183 | Density | ISO 1183 | g/cm^3 | 1.59 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Deflection Temperature under Load Deflection Temperature under Load/ISO 75-1/-2 | Deflection temperature under load (1.80MPa) | ISO 75-1/-2 | ℃ | 236 | - |
Linear expansion coefficient (MD) Linear expansion coefficient (MD)/ISO 11359-1/-2 | Linear expansion coefficient (parallel) | ISO 11359-1/-2 | x10^-5/℃ | 1.4 | - |
Linear expansion coefficient (TD) Linear expansion coefficient (TD)/ISO 11359-1/-2 | Linear expansion coefficient (right angle) | ISO 11359-1/-2 | x10^-5/℃ | 5.5 | - |
Flammability Flammability/IEC 60695-11-10 | Flammability | IEC 60695-11-10 | NaN | 1.5mm |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile breaking stress Tensile breaking stress/ISO 527-1/-2 | Breaking stress (when completely dry) | ISO 527-1/-2 | MPa | 250 | - |
Breaking stress (when humidified) | ISO 527-1/-2 | MPa | 215 | - | |
Tensile strain at break Tensile strain at break/ISO 527-1/-2 | Breaking strain (when completely dry) | ISO 527-1/-2 | % | 2.8 | - |
Breaking strain (when humidity controlled) | ISO 527-1/-2 | % | 3.2 | - | |
Tensile Modulus Tensile Modulus/ISO 527-1/-2 | Tensile modulus (when completely dry) | ISO 527-1/-2 | MPa | 16500 | - |
Tensile modulus (when conditioned) | ISO 527-1/-2 | MPa | 16300 | - | |
Flexural modulus Flexural modulus/ISO 178 | Flexural modulus (when completely dry) | ISO 178 | MPa | 15000 | - |
Charpy impact strength Charpy impact strength/ISO 179/1eA | Notched Charpy impact strength (23°C) (when completely dry) | ISO 179/1eA | kJ/m^2 | 15 | - |
Notched Charpy impact strength (-40℃) (absolutely dry) | ISO 179/1eA | kJ/m^2 | 14 | - | |
Charpy impact strength (23℃) (when not exposed to heat) | ISO 179/1eU | kJ/m^2 | 95 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tracking resistance Tracking resistance/IEC60112 | Tracking resistance (when completely dry) | IEC60112 | 600 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Resin temperature Resin temperature/- | Optimum resin temperature | - | ℃ | 290 | - |
Drying conditions Drying conditions/- | Drying temperature | - | ℃ | 100 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Filler Content Filler Content/ | Filler Content | % | 50 | GF |
| Key Features |
|---|
Heat resistance, impact resistance, high rigidity |