| Manufacturer | Toyo Styrene Co., Ltd. |
| Resin Name | PS |
| Product Name | Toyo Styrol HI |
| ISO Material Code | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Vicat softening temperature Vicat softening temperature/JIS K7206 | Bit softening temperature (50N load) | JIS K7206 | ℃ | 90 | - |
Deflection Temperature under Load Deflection Temperature under Load/JIS K7191 | Deflection temperature under load (1.8 MPa load) | JIS K7191 | ℃ | 71 | - |
Flammability Flammability/UL 94 | Flammability | UL 94 | NaN | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile Yield Stress Tensile Yield Stress/JIS K7161 | Tensile Yield Stress | JIS K7161 | MPa | 25 | - |
Tensile strain at break Tensile strain at break/JIS K7162 | Tensile strain at break | JIS K7162 | % | 50 | - |
Bending strength Bending strength/JIS K7171 | Bending strength | JIS K7171 | MPa | 44 | - |
Flexural modulus Flexural modulus/JIS K7171 | Flexural modulus | JIS K7171 | MPa | 2150 | - |
Charpy impact strength Charpy impact strength/JIS K7111 | Charpy impact strength | JIS K7111 | kJ/m^2 | 10 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
MFR MFR/JIS K7210 | MFR | JIS K7210 | g/10min | 11 | - |
| Key Features |
|---|
HIPS, for injection molding, good flow |