| Manufacturer | BASF Japan Ltd. |
| Resin Name | PBT |
| Product Name | Ultradur |
| ISO Material Code | >PBT-GB30< |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO 1183 | Density | ISO 1183 | g/cm^3 | 1.53 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Deflection Temperature under Load Deflection Temperature under Load/ISO 75-1,2 | Deflection temperature under load (1.8MPa) | ISO 75-1,2 | ℃ | 75 | - |
Deflection temperature under load (0.45MPa) | ISO 75-1,2 | ℃ | 175 | - | |
Linear expansion coefficient Linear expansion coefficient/ISO 11359-2 | Linear expansion coefficient | ISO 11359-2 | ×10^-5/℃ | 7.5 | - |
Flammability Flammability/UL 94 | Flammability | UL 94 | NaN | 0.75mm (minimum thickness) |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile strain at break Tensile strain at break/ISO 527-1,2 | Tensile strain at break | ISO 527-1,2 | % | 5 | - |
Charpy impact strength Charpy impact strength/ISO 179-1 | Charpy (notched) | ISO 179-1 | kJ/m^2 | 3 | - |
Tensile strength Tensile strength/ISO 527-1,2 | Tensile (yield) strength | ISO 527-1,2 | MPa | 50 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Dielectric constant Dielectric constant/IEC 60250 | Dielectric constant | IEC 60250 | 3.8 | - | |
Dielectric Strength Dielectric Strength/IEC 60243-1 | Withstand voltage (dielectric breakdown strength) | IEC 60243-1 | kV/mm | 37 | - |
Tracking resistance Tracking resistance/UL 746A | CTI | UL 746A | UL Index | 225 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Mold shrinkage rate MD Mold shrinkage rate MD/Company method | Mold shrinkage (machine direction MD) | Company method | 1.7 | - | |
Mold shrinkage rate TD Mold shrinkage rate TD/Company method | Mold shrinkage (transverse direction TD) | Company method | % | 1.7 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
30 | GB |
| Color |
|---|
Black |
| Main Applications |
|---|
General injection, industrial materials, consumer goods, etc. |
| Key Features |
|---|
Injection molding, low warpage, 30% reinforced glass beads |