| Manufacturer | Celanese Corporation |
| Resin Name | PA66 |
| Product Name | Zytel |
| ISO Material Code | PA66-F |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO 1183 | Density (dry) | ISO 1183 | g/cm^3 | 1.04 | - |
Water absorption Water absorption/ISO 62 | Equilibrium water absorption (2mm) (when absorbing moisture) | ISO 62 | % | 1.4 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Deflection Temperature under Load Deflection Temperature under Load/ISO 75-1/-2 | Deflection temperature under load (1.80 MPa) (when completely dry) | ISO 75-1/-2 | ℃ | 50 | - |
Deflection temperature under load (0.45 MPa) (when completely dry) | ISO 75-1/-2 | ℃ | 68 | - | |
Melting point Melting point/ISO 11357-1/-3 | Melting temperature (10℃/min) (when completely dry) | ISO 11357-1/-3 | ℃ | 263 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile strain at break Tensile strain at break/ISO 527-1/-2 | Breaking strain (when completely dry) | ISO 527-1/-2 | % | 50 | - |
Breaking strain (at 23℃ 50% RH equilibrium water absorption) | ISO 527-1/-2 | % | 50 | - | |
Tensile Modulus Tensile Modulus/ISO 527-1/-2 | Tensile modulus (when completely dry) | ISO 527-1/-2 | MPa | 900 | - |
Tensile modulus (at 23℃ 50% RH equilibrium water absorption) | ISO 527-1/-2 | MPa | 440 | - | |
Flexural modulus Flexural modulus/ISO 178 | Flexural modulus (when completely dry) | ISO 178 | MPa | 900 | - |
Charpy impact strength Charpy impact strength/ISO 179/1eA | Notched Charpy impact strength (23°C) (when completely dry) | ISO 179/1eA | kJ/m^2 | 105 | - |
Notched Charpy impact strength (-40℃) (absolutely dry) | ISO 179/1eA | kJ/m^2 | 30 | - | |
Izod impact strength Izod impact strength/ISO 180/1A | Izod impact strength, notched (23°C) (when completely dry) | ISO 180/1A | kJ/m^2 | 95 | - |
Izod impact strength, notched (-40°C) (absolutely dry) | ISO 180/1A | kJ/m^2 | 25 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Resin temperature Resin temperature/ | Optimum resin temperature | ℃ | 285 | - | |
Mold Temperature Mold Temperature/ | Optimal Mold Temperature | ℃ | 60 | - | |
Drying conditions Drying conditions/ | Drying temperature | ℃ | 80 | 2 - 4h |
Copyright© 2025 PlaBase. All Rights Reserved.