| Manufacturer | Celanese Corporation |
| Resin Name | PA |
| Product Name | Zytel |
| ISO Material Code | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO 1183 | Density | ISO 1183 | g/cm^3 | 1.58 | - |
Water absorption Water absorption/ISO 62 | Balanced water absorption (2mm) | ISO 62 | % | 0.6 | - |
Water absorption (immersion, 24h) | ISO 62 | % | 0.3 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Deflection Temperature under Load Deflection Temperature under Load/ISO 75-1/-2 | Deflection temperature under load (1.80MPa) | ISO 75-1/-2 | ℃ | 192 | - |
Melting point Melting point/ISO 11357-1/-3 | Melting temperature (10℃/min) | ISO 11357-1/-3 | ℃ | 201 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile breaking stress Tensile breaking stress/ISO 527-1/-2 | Breaking stress (when completely dry) | ISO 527-1/-2 | MPa | 230 | - |
Breaking stress (when humidified) | ISO 527-1/-2 | MPa | 210 | - | |
Tensile strain at break Tensile strain at break/ISO 527-1/-2 | Breaking strain (when completely dry) | ISO 527-1/-2 | % | 2.5 | - |
Breaking strain (when humidity controlled) | ISO 527-1/-2 | % | 2.3 | - | |
Tensile Modulus Tensile Modulus/ISO 527-1/-2 | Tensile modulus (when completely dry) | ISO 527-1/-2 | MPa | 17000 | - |
Tensile modulus (when conditioned) | ISO 527-1/-2 | MPa | 15000 | - | |
Flexural modulus Flexural modulus/ISO 178 | Flexural modulus (when conditioned) | ISO 178 | MPa | 14000 | - |
Charpy impact strength Charpy impact strength/ISO 179/1eA | Notched Charpy impact strength (23°C) (humidified) | ISO 179/1eA | kJ/m^2 | 24 | - |
Charpy impact strength (23℃) (when completely dry) | ISO 179/1eU | kJ/m^2 | 100 | - | |
Charpy impact strength (23℃) (humidified) | ISO 179/1eU | kJ/m^2 | 80 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tracking resistance Tracking resistance/IEC 60112 | Tracking resistance (when completely dry) | IEC 60112 | 600 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Resin temperature Resin temperature/ | Optimum resin temperature | ℃ | 250 | - | |
Drying conditions Drying conditions/ | Drying temperature | ℃ | 100 | - |