| Manufacturer | Solvay Specialty Polymers Japan Co., Ltd. |
| Resin Name | PA |
| Product Name | Ixef |
| ISO Material Code | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO1183 | Density | ISO1183 | g/cm^3 | 1.34 | - |
Water absorption Water absorption/ISO62 | Water absorption rate (23℃, 24hr) | ISO62 | % | 0.22 | - |
Water absorption (balance, 65%RH) | Internal Method | % | 2 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Deflection Temperature under Load Deflection Temperature under Load/ISO75-2/A | Deflection temperature under load (1.8MPa, no annealing treatment) | ISO75-2/A | ℃ | 230 | - |
Flammability Flammability/UL94 | Flammability | UL94 | NaN | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile Yield Stress Tensile Yield Stress/ISO527-2 | Tensile Yield Strength | ISO527-2 | MPa | 250 | - |
Tensile strain at break Tensile strain at break/ISO527-2 | Tensile elongation at break | ISO527-2 | % | 1.3 | - |
Tensile Modulus Tensile Modulus/ISO527-2 | Tensile Modulus | ISO527-2 | MPa | 26000 | - |
Bending strength Bending strength/ISO178 | Bending stress | ISO178 | MPa | 360 | - |
Flexural modulus Flexural modulus/ISO178 | Flexural modulus | ISO178 | MPa | 23000 | - |
Charpy impact strength Charpy impact strength/ISO179 | Charpy impact strength (unnotched) | ISO179 | kJ/m^2 | 36 | - |
Charpy impact strength (notched) | ISO179 | kJ/m^2 | 3.6 | - | |
Izod impact strength Izod impact strength/ASTMD256 | Izod impact strength (unnotched) | ASTMD256 | J/m | 450 | - |
Izod impact strength (notched) | ASTMD256 | J/m | 59 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Volume resistivity Volume resistivity/ASTMD257 | Volume resistivity | ASTMD257 | Ω・cm | NaN | - |
Tracking resistance Tracking resistance/IEC60112 | Tracking resistance | IEC60112 | V | 600 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Mold shrinkage rate MD Mold shrinkage rate MD/Internal Method | Mold shrinkage rate MD | Internal Method | % | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Resin temperature Resin temperature/ | Resin temperature | ℃ | - | ||
Mold Temperature Mold Temperature/ | Mold Temperature | ℃ | - | ||
Drying conditions Drying conditions/ | Drying conditions | ℃ | 120 | 0.50-1.5hr |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Filler Content Filler Content/ | Filler content (CF) | % | 30 | - |
| Color |
|---|
Black |
| Main Applications |
|---|
Home appliance parts,Home appliances,Automobiles,Auto electronic parts,Auto parts,Bushings,Cameras,Mobile phones,Electrical/Electronic,Furniture,Gears,Industrial applications,Lawn mowers,Machinery/Machine parts,Metal replacement,Power supplies/Other tools |