| Manufacturer | Solvay Specialty Polymers Japan Co., Ltd. |
| Resin Name | PPA |
| Product Name | Amodel |
| ISO Material Code | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ISO1183/A | Density | ISO1183/A | g/cm^3 | 1.57 | - |
Water absorption Water absorption/ASTMD570 | Water absorption rate (24hr) | ASTMD570 | % | 0.37 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Deflection Temperature under Load Deflection Temperature under Load/ISO75-2/Af | Deflection temperature under load (1.8MPa, no annealing treatment) | ISO75-2/Af | ℃ | 297 | - |
Linear expansion coefficient (flow) Linear expansion coefficient (flow)/ASTME831 | Linear expansion coefficient (flow, 0 to 100℃) | ASTME831 | ×10^-5/℃ | 2 | - |
Linear expansion coefficient (flow, 100 to 200℃) | ASTME831 | ×10^-5/℃ | 1.5 | - | |
Linear expansion coefficient (right angle) Linear expansion coefficient (right angle)/ASTME831 | Linear expansion coefficient (right angle, 0 to 100℃) | ASTME831 | ×10^-5/℃ | 7.6 | - |
Linear expansion coefficient (right angle, 100 to 200℃) | ASTME831 | ×10^-5/℃ | 12 | - | |
Melting point Melting point/ISO11357-3 | Melting point | ISO11357-3 | ℃ | 327 | - |
Melting point | ASTMD570 | ℃ | 327 | - | |
Flammability Flammability/UL94 | Flammability | UL94 | NaN | 3.2mm |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile breaking stress Tensile breaking stress/ISO527-2 | Tensile strength at break (23℃) | ISO527-2 | MPa | 225 | - |
Tensile strength at break (200℃) | ISO527-2 | MPa | 70 | - | |
Tensile strength at break (230℃) | ISO527-2 | MPa | 60 | - | |
Tensile strain at break Tensile strain at break/ISO527-2 | Tensile elongation at break (23℃) | ISO527-2 | % | 1.8 | - |
Tensile elongation at break (200℃) | ISO527-2 | % | 6.1 | - | |
Tensile elongation at break (230℃) | ISO527-2 | % | 6.3 | - | |
Tensile Modulus Tensile Modulus/ISO527-2 | Tensile Modulus | ISO527-2 | MPa | 16400 | - |
Bending strength Bending strength/ISO178 | Bending stress (23℃) | ISO178 | MPa | 325 | - |
Flexural modulus Flexural modulus/ISO178 | Flexural modulus (23℃) | ISO178 | MPa | 14500 | - |
Charpy impact strength Charpy impact strength/ISO179/1eU | Charpy impact strength (unnotched, 23℃) | ISO179/1eU | kJ/m^2 | 80 | - |
Charpy impact strength (notched, 23℃) | ISO179/1eA | kJ/m^2 | 11 | - | |
Izod impact strength Izod impact strength/ISO180/1U | Izod impact strength (unnotched, 23℃) | ISO180/1U | kJ/m^2 | 65 | - |
Izod impact strength (notched, 23℃) | ISO180/1A | kJ/m^2 | 10 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Volume resistivity Volume resistivity/ASTMD257 | Volume resistivity | ASTMD257 | Ω・cm | NaN | - |
Dielectric constant Dielectric constant/ASTMD150 | Dielectric constant (60Hz) | ASTMD150 | 3.8 | - | |
Dielectric constant (1MHz) | ASTMD150 | 3.6 | - | ||
Dielectric loss tangent Dielectric loss tangent/ASTMD150 | Dielectric tangent (60Hz) | ASTMD150 | 0.004 | - | |
Dielectric tangent (1MHz) | ASTMD150 | 0.012 | - | ||
Dielectric Strength Dielectric Strength/ASTMD149 | Dielectric strength (1.60mm) | ASTMD149 | kV/mm | 20 | - |
Tracking resistance Tracking resistance/UL746 | Tracking resistance | UL746 | V | 600 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Mold shrinkage rate MD Mold shrinkage rate MD/ASTMD955 | Mold shrinkage rate MD | ASTMD955 | % | 0.4 | - |
Mold shrinkage rate TD Mold shrinkage rate TD/ASTMD955 | Mold shrinkage rate TD | ASTMD955 | % | 0.8 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Resin temperature Resin temperature/ | Resin temperature | ℃ | - | ||
Mold Temperature Mold Temperature/ | Mold Temperature | ℃ | - | ||
Drying conditions Drying conditions/ | Drying conditions | ℃ | 120 | 4.0hr |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Filler Content Filler Content/ | Filler content (GF) | % | 45 | - |
| Color |
|---|
Black |
| Main Applications |
|---|
Automobiles, Automobile parts, Metal replacements |
| Key Features |
|---|
Chemical resistance, creep resistance, fast molding cycle, good dimensional stability, high rigidity, thermal stability, high heat resistance, high strength, hot water moldability, laser weldable, low moisture absorption, lubrication |
Copyright© 2026 PlaBase. All Rights Reserved.