| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Density Density/ASTM D792 | Density/Specific Gravity | ASTM D792 | g/cm^3 | 1.67 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Deflection Temperature under Load Deflection Temperature under Load/ASTM D648 | Deflection temperature under load (1.8MPa, no annealing) | ASTM D648 | ℃ | 262 | - |
Linear expansion coefficient (flow) Linear expansion coefficient (flow)/ASTM D696 | Linear expansion coefficient, parallel | ASTM D696 | ×10^-5/℃ | 0.6 | - |
Linear expansion coefficient (right angle) Linear expansion coefficient (right angle)/ASTM D696 | Linear expansion coefficient, vertical | ASTM D696 | ×10^-5/℃ | 2.2 | - |
Flammability Flammability/UL 94 | Flammability Rating | UL 94 | NaN | 0.78mm |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Tensile strain at break Tensile strain at break/ISO 527-2 | Tensile elongation (break point, 23℃) | ISO 527-2 | % | 1.6 | - |
Tensile elongation (break point) | ASTM D638 | % | 4.6 | - | |
Bending strength Bending strength/ISO 178 | Bending strength (23℃) | ISO 178 | MPa | 162 | - |
Bending strength | ASTM D790 | MPa | 171 | - | |
Flexural modulus Flexural modulus/ISO 178 | Flexural modulus (23℃) | ISO 178 | MPa | 14100 | - |
Flexural modulus | ASTM D790 | MPa | 13300 | - | |
Charpy impact strength Charpy impact strength/ISO 179 | Charpy impact strength (notched, 23℃) | ISO 179 | kJ/m^2 | 4 | - |
Izod impact strength Izod impact strength/ASTM D256 | Notched Izod impact | ASTM D256 | J/m | 61 | - |
Tensile strength Tensile strength/ISO 527-2 | Tensile strength (23℃) | ISO 527-2 | MPa | 131 | - |
Tensile strength | ASTM D638 | MPa | 145 | - |
Blurred items can be viewed by registering or logging in.
Blurred items can be viewed by registering or logging in.
| Property | Details | Inspection Methods | Unit | Value | Note |
|---|---|---|---|---|---|
Mold shrinkage rate MD Mold shrinkage rate MD/Toray method | Mold shrinkage, parallel: 1.00mm (80×80×1mm) | Toray method | % | -0.11 | - |
Mold shrinkage rate TD Mold shrinkage rate TD/Toray method | Molding shrinkage, vertical: 1.00mm (80×80×1mm) | Toray method | % | 0.91 | - |
| Main Applications |
|---|
Connector |
| Key Features |
|---|
GF + inorganic filler reinforcement, heat resistance, good flow |